Showing 1 - 20 results of 25 for search 'C.', query time: 0.35s Refine Results
  1. 1
    ... form a clinker with high contents of α’L-C2S modification. Microcalorimetric measurements show a...
    Get full text
    Online
  2. 2
    ... the two days of cured, cubic aluminate C3AH6), and AH3 polymorphs are formed, instead of the usual...
    Get full text
    Online
  3. 3
  4. 4
    ... lying in the range of CaO = 69,5-70,1; P2O5= 16,2-19,5; SiO2 = 11,1-13,6 (wt%) give, at 1000 °C...
    Get full text
    Online
  5. 5
    ... the formation of HAp with β-C2S and C5PS, using some compositions in the rich lime portion of the system CaO-SiO...
    Get full text
    Online
  6. 6
    by Puertas, F., Amat, T., Vázquez, T.
    Published 2000
    ... furnace slag activated with NaOH 2M (room temperature, 22 ºC); fly ash activated with NaOH 8M, cured at 85...
    Get full text
    Online
  7. 7
    ...Sulfoaluminate belite clinkers by burning raw at moderate temperatures near 1250 °C were...
    Get full text
    Online
  8. 8
    ... of the hydrated cement paste reaction product. The C-S-H gel formed in these pastes differed in quantity, which...
    Get full text
    Online
  9. 9
    ... reaction between the barium carbonate and the C3A of the clinker appears. The BaCO3 reveals a retardant...
    Get full text
    Online
  10. 10
  11. 11
    ... composition of clinkers. New phases like 2 CaO.Mn02 and Ca2AIMnO5 are developed and C3A formation can...
    Get full text
    Online
  12. 12
    by Puertas, F., Vázquez, T.
    Published 2001
    ... (specially, alite phase), b) The ettringite formation is affected by the nature of the admixture. c)A...
    Get full text
    Online
  13. 13
  14. 14
  15. 15
  16. 16
  17. 17
  18. 18
  19. 19
  20. 20