61 - 80 toradh á dtaispeáint as 376 toradh san iomlán ar an gcuardach 'M.', am iarratais: 0.33s Beachtaigh na torthaí
  1. 61
    de réir SILVIA LORENA MONTES FONSECA
    Foilsithe / Cruthaithe 2012
    ... (P-CNTs) CNTs by two different methods: (1) reflux with 3M HNO3 and (2) sonication in H2SO4/HNO3...
    Faigh an téacs iomlán
    info:eu-repo/semantics/article
  2. 62
  3. 63
  4. 64
  5. 65
  6. 66
  7. 67
    de réir JUAN ANDRES AGUILAR MARTINEZ
    Foilsithe / Cruthaithe 2003
    ... porosity diminishes with decreasing particle size. Using 20 μm powders, none of the two types of SiC...
    Faigh an téacs iomlán
    info:eu-repo/semantics/conferenceProceedings
  8. 68
    de réir IGNACIO RAMIRO MARTIN DOMINGUEZ
    Foilsithe / Cruthaithe 2013
    ... solar heating area is about 338 m2, using 195 flat-coated solar heaters, copper tube and aluminum fin...
    Faigh an téacs iomlán
    info:eu-repo/semantics/conferencePoster
  9. 69
    de réir ENEFTALI FLORES GARCIA
    Foilsithe / Cruthaithe 2015
    .... CuCl2 (0.1M), 15 ml. Na3C3H5O (COO)3 (0.5M), “x” ml. KOH (0.5M), “y” ml. buffer base borato, 7.5 ml. CS...
    Faigh an téacs iomlán
    info:eu-repo/semantics/masterThesis
  10. 70
    de réir BEATRIZ ALEJANDRA GARCIA TORRES
    Foilsithe / Cruthaithe 2017
    ... libre de fracturas en esferas con diámetros de hasta 15 μm con área superficial específica de 560 m2/g...
    Faigh an téacs iomlán
    info:eu-repo/semantics/doctoralThesis
  11. 71
    ... preparado a partir de una solución acuosa de AgNO3 y H2Pt(NO2)2SO4 la cual se adiciona a 10 mL of toluene...
    Faigh an téacs iomlán
    info:eu-repo/semantics/conferenceProceedings
  12. 72
    de réir LUZ OLIVIA LEAL QUEZADA
    Foilsithe / Cruthaithe 2011
    ... of them was employed 5% (v/v) H2O2 as an oxidant with 1.5% (m/v) KBH4 as a reducing agent and 1.5% (v/v...
    Faigh an téacs iomlán
    info:eu-repo/semantics/conferenceProceedings
  13. 73
    ... M(H) measurements reveal the coexistence of a strong antiferromagnetic (AFM) signal and a...
    Faigh an téacs iomlán
    info:eu-repo/semantics/article
  14. 74
    de réir LUZ OLIVIA LEAL QUEZADA
    Foilsithe / Cruthaithe 2015
    .... Plumbane was generated through two methods: (1) 5% (v/v) H2O2 was employed as oxidant with 1.5% (m/v) KBH4...
    Faigh an téacs iomlán
    info:eu-repo/semantics/article
  15. 75
    de réir JUAN ANDRES AGUILAR MARTINEZ
    Foilsithe / Cruthaithe 2010
    ...In this work the degradation of metal/composite (M/C) interfaces in Al-Mg- Si/SiCp composites...
    Faigh an téacs iomlán
    info:eu-repo/semantics/conferenceProceedings
  16. 76
  17. 77
  18. 78
    de réir JOSE TRINIDAD ELIZALDE GALINDO, JOSE ANDRES MATUTES AQUINO
    Foilsithe / Cruthaithe 2005
    .... The surface velocity of the Cu roll was varied between 25 and 48.5 m/s. Magnetic anisotropy was observed...
    Faigh an téacs iomlán
    info:eu-repo/semantics/article
  19. 79
  20. 80
    de réir Lorena Alvarez Contreras, MINERVA GUERRA BALCAZAR
    Foilsithe / Cruthaithe 2018
    ... betaina presenta la mayor densidad de corriente (55.16 mA cm-2) a una concentración de 1.5 M etanol...
    Faigh an téacs iomlán
    info:eu-repo/semantics/article